BiFeO3–BaTiO3 lead-free piezoelectric ceramics have been studied for their application to sensors and actuators. The high strain and piezoelectric actuator coefcient (d33*) are observed in tetragonal 0.60BiFeO3–0.40BaTiO3 ceramic with heat treated single-phase rutile titanium dioxide (TiO2) powders than in ceramic with commercial mixed-phase with rutile and anatase TiO2. The optimized sintering temperature is 1010 °C with the quenching process. The increase of the grain size in microstructure, higher tetragonal phase volume fraction, and higher tetragonality are observed in ceramic with rutile TiO2 than in ceramic with commercial TiO2. The maximum strain is 0.316%, and d33* is 576 pm/V. A high Curie phase transition temperature of 355 °C is measured with the maximum dielectric constant (εr , max) about 30% higher than that of ceramic with commercial TiO2. It is found that the single-phase starting material is important to improve piezoelectric, ferroelectric, and dielectric properties in lead-free piezoelectric ceramics.