주요 논문
5
*2026년 기준 최근 7년 이내 논문에 한해 Impact Factor가 표기됩니다.
1
Article
|
·
인용수 0
·
2025Landau-Devonshire theory-based phase diagram of the bismuth ferrite and barium titanate solid solution
Hae In Choi, Myang Hwan Lee, Won-Jeong Kim, Tae Kwon Song
IF 2.8 (2025)
Current Applied Physics
The development of high-performance, lead-free piezoelectric ceramics is essential for modern sensor and actuator applications. Bismuth ferrite-based solid solutions, like (1-x)BiFeO3-xBaTiO3 (BF-BT), are promising due to their high Curie temperature and high piezoelectric performance, but ambiguities persist regarding their phase transitions and the exact location of the morphotropic phase boundary (MPB), where piezoelectric properties are maximized. This study resolves these issues by applying Landau-Devonshire theory to construct a comprehensive phase diagram for the BF-BT system. By calculating the free energy density landscape, our theoretical model accurately reproduces the material's composition-dependent properties. The resulting phase diagram agrees well with experimental observations, predicting a coexistence of rhombohedral and tetragonal phases near x = 0.33. And our calculations identify the MPB at a composition of x = 0.375, consistent with the experimentally reported range. These findings highlight the link between phase structure and piezoelectric performance.
https://doi.org/10.1016/j.cap.2025.10.009
Phase boundary
Phase diagram
Tetragonal crystal system
Piezoelectricity
Solid solution
Barium titanate
Curie temperature
Bismuth ferrite
2
Article
|
·
인용수 6
·
2025Hard Piezoelectric Properties of MnCO3-Doped Lead-Free BiFeO3–BaTiO3 Ceramics with High Curie Temperature
M. H. Lee, Hae In Choi, Da Jeong Kim, Sang Woo Lee, Yu Bin Park, Sang Mo Yang, Tae Kwon Song
IF 7.8 (2025)
ACS Applied Materials & Interfaces
Lead-free BiFeO 3 –BaTiO 3 (BF–BT) ceramics show high potential for piezoelectric sensors, actuators, and high-power transducers owing to their excellent piezoelectric properties and high Curie temperatures ( T C ). Hard piezoelectric material used in high-power transducer applications must exhibit a high mechanical quality factor ( Q m ), high coercive field ( E C ), high T C, and low dielectric loss (tan δ). Herein, the effects of doping in BF–BT ceramics with the hard acceptor dopant Mn 2+ are investigated to enhance their hard piezoelectric properties. The 0.8Bi 1.02 (Fe 1– x Mn x )O 3 –0.2BaTiO 3 ( x = 0, 0.005, 0.01, 0.015, and 0.02) ceramics are prepared using solid-state reaction and water-quenching processes. The increasing of the Mn 2+ content in BF–BT ceramics boosts the piezoelectric charge sensor coefficient ( d 33 ), Q m, T C, planar piezoelectric coupling factor ( k p ), E C, and internal bias field ( E i ), reaching their maximum values at x = 0.01 ( d 33 = 74 pC/N, Q m = 757, T C = 652 °C, k p = 0.26, E C = 65 kV/cm, and E i = 6.2 kV/cm) with the lowest loss (tan δ = 0.009). Then, the hard piezoelectric properties deteriorate gradually with an increasing Mn content. The ferroelectric domain structure and dynamics are compared to defect-related ferroelectric and piezoelectric properties. These results show that the hard acceptor Mn 2+ in the BF–BT ceramics improves the performance of lead-free ceramics for high-power piezoelectric transducers in high-temperature environments.
https://doi.org/10.1021/acsami.5c02859
Materials science
Curie temperature
Piezoelectricity
Ceramic
Doping
Condensed matter physics
Lead (geology)
Ferroelectricity
Curie
Dielectric
3
Article
|
인용수 5
·
2024Ferroelectric Polarization Dependent Piezoelectric Hardening in BiFeO 3 ‐BaTiO 3 Lead‐Free Ceramics
M. H. Lee, Hae In Choi, Da Jeong Kim, Ji Su Kim, Sang Woo Lee, Yu Bin Park, Sang Mo Yang, Tae Kwon Song
IF 5.3 (2024)
Advanced Electronic Materials
Abstract The relation between the improvement of mechanical quality factor ( Q m ) and internal electric field ( E i ) generated during the aging process in lead‐free piezoelectric BiFeO 3 ‐BaTiO 3 ceramics is investigated for hard piezoelectric application of power transducers. The change of built‐in E i depends on the ferroelectric polarization ( P ) direction during the aging process. For the aging process with P parallel to E i , Q m and E i increases but Q m and E i decreases with P antiparallel to E i . These results are attributed to the migration of defects by depolarization fields and domain‐wall pinning. This work provides the systematic guidance to develop high‐power piezoelectric transducers with lead‐free ceramics.
https://doi.org/10.1002/aelm.202300902
Materials science
Piezoelectricity
Ferroelectricity
Polarization (electrochemistry)
Ceramic
Coercivity
Work hardening
Composite material
Hardening (computing)
Condensed matter physics
4
Article
|
인용수 21
·
2023Hard piezoelectric properties of lead‐free BiFeO 3 –BaTiO 3 ceramics
Myang Hwan Lee, Hae In Choi, Da Jeong Kim, Ji Su Kim, Tae Kwon Song
IF 3.5 (2023)
Journal of the American Ceramic Society
Abstract Hard piezoelectric properties are investigated in lead‐free BiFeO 3 –BaTiO 3 (BF–BT) ceramics. Rhombohedral (R) phase ceramics of (1 – x )BF– x BT ( x = 0.20–0.30) were prepared using a conventional solid‐state reaction and water‐quenching process. The R structure is observed in x = 0.20–0.275, and the R and tetragonal phases coexist at x = 0.30. The piezoelectric charge sensor coefficient ( d 33 ) and electromechanical planar coupling factor ( k p ) increase with increasing BT content, whereas the mechanical quality factor ( Q m ) decreases. The x = 0.20 ceramic shows the best hard piezoelectric properties: the highest Q m = 403 and the highest T C = 607°C. In contrast, x = 0.30 ceramic shows soft piezoelectric properties: d 33 = 301 pC/N and k p = 0.33 with T C = 510°C. These results show that the BF–BT system in R‐phase‐rich region has good hard piezoelectric properties for transducer applications.
https://doi.org/10.1111/jace.19439
Piezoelectricity
Materials science
Ceramic
Tetragonal crystal system
Piezoelectric coefficient
Electromechanical coupling coefficient
Quenching (fluorescence)
Phase (matter)
Analytical Chemistry (journal)
Mineralogy
5
Article
|
·
인용수 17
·
2022Bipolar cycling effects in BiFeO3–BaTiO3 piezoelectric ceramics
Kim Da Jeong, Lee Myang Hwan, Choi Hai In, Jung Yeon-Gil, Lee Soonil, Song Tae Kwon
IF 2.4 (2022)
Current Applied Physics
BiFeO3–BaTiO3 (BF-BT) lead-free piezoelectric system has been paid much attention due to good piezoelectric properties and high Curie temperature. Poling is a process to align ferroelectric domains and increase the piezoelectric coefficients. During the poling process, unipolar direct current (dc) electric fields were applied conventionally, but recently bipolar alternating current (ac) cycling was reported to improve piezoelectric properties in rhombohedral structure piezoelectric materials. We investigated the effects of dc-poling and ac-cycling in BF-BT ceramics. The d33 increased from 210 pC/N with dc-poling to 240 pC/N with ac-cycling in the morphotropic phase boundary region of BF-BT with domain engineering. This improvement of piezoelectric properties with ac-cycling was consistent with the structural evolution related to ferroelectric domains.
https://doi.org/10.1016/j.cap.2022.09.004
Poling
Piezoelectricity
Materials science
Ferroelectricity
Curie temperature
Phase boundary
Ceramic
Piezoelectric coefficient
Cycling
Composite material